Welding Instruction |
|||||||||
(1) Dry the electrodes at 300-350°C for 30-60 minutes before use. (2) Preheat is not needed. Use low current to prevent overheat. (3) Keep good ventilation during welding. |
|||||||||
Typical Chemical Composition of Weld Metal (wt. %) |
|||||||||
C |
Si |
Mn |
Ni |
||||||
0.680 |
0.50 |
13.51 |
3.71 |
||||||
Typical Hardness of Weld Metal |
|||||||||
Hardness Condition |
Vicker’s hardness (HV) |
Rockwell’s hardness (HRC) |
Shore’s hardness (HS) |
||||||
Interpass temp.≤150°C |
190 |
8.5 |
28 |
||||||
Work-hardened |
430 |
43 |
58 |
||||||
Size and Suggested Operating Range (AC or DC+) |
|||||||||
Diameter x Length(mm) |
3.2x350 |
4.0x400 |
5.0x400 |
||||||
Amp |
90~140 |
140~190 |
190~250 |